Meaning
Standardized testing protocols measure the resistance of semi-crystalline polymers to slow crack growth in the presence of a surfactant. iso 16770 utilizes a notched specimen subjected to a constant tensile load while submerged in a chemical reagent. This method accelerates the failure time compared to air-based tests.
Stress Application
Machined notches on all four sides of a test bar create a complex stress state that mimics field failures. The application of load in iso 16770 targets the tie molecules that span the amorphous regions between crystalline lamellae. This mechanism reveals the inherent strength of the resin against brittle fracture.
Surface Tension
Chemical environments lower the energy required for the initiation of micro-voids at the notch tip. Testing according to iso 16770 often uses nonylphenol ethoxylates to simulate the aggressive fluids encountered in pipe or container applications. The rate of crack propagation provides a ranking of different resin grades.
Failure Identification
Creep rupture time is the primary metric for evaluating the durability of the material under load. High density polyethylene grades tested via iso 16770 show a distinct transition from ductile to brittle behavior. This value helps designers select materials for long term structural integrity in harsh environments.