Meaning
Resistance encountered by the advancing melt front as it compresses the residual air and gases within the steel mold during the injection phase. Inadequate venting or excessively high injection speeds escalate cavity backpressure, which can halt the flow front prematurely. The resulting restriction can prevent the melt from filling thin-wall regions, causing short shots.
Venting Performance
Resistance of the venting channels determines the rate at which gas can escape from the impression. When cavity backpressure exceeds the injection pressure limit of the molding machine, the flow front stalls. This phenomenon generates severe localized compression, heating the trapped gas to temperatures that burn the polymer.
Moulders often encounter this when transitioning from virgin to recycled resins, which can outgas more during processing and require frequent cleaning of the vent paths.
Defect Prevention
Venting defects such as diesel burns or incomplete filling are directly tied to uncontrolled gas resistance during high-speed injection. Monitoring the pressure inside the tool provides a method to adjust the clamping force or clean clogged vents. Regular maintenance of the ejector pin clearances ensures a clear path for gas escape.
Machine Adjustment
Process engineers reduce the fill rate or apply a vacuum to lower the gas resistance. If the cavity backpressure remains high, modifying the gate location or increasing vent depth resolves the issue.