Meaning
Incorporation of microscopic pockets of gas or air into a polymer melt during the plastication or injection phase creates tiny internal cavities in the solidified part. This physical process, termed microvoid entrainment, occurs when high shear forces or improper venting trap air or volatile gases within the melt flow. It reduces the mechanical strength and density of the finished product.
The phenomenon is most critical in thick-walled parts and high-viscosity resins where the bubbles cannot migrate to the surface.
Entrainment Mechanism
Screw speed and back pressure during the dosing phase affect the amount of trapped gas. When back pressure is too low, microvoid entrainment happens because the screw fails to compress the melting resin sufficiently. These microvoids also form when the melt front flows too fast over irregular mold textures, trapping pockets of air.
The gas remains trapped as the polymer cools.
Part Performance
Mechanical failure occurs under low load when microvoids are present. This microvoid entrainment lowers the tensile strength and impact resistance of the plastic parts. It is particularly damaging in transparent optical parts because it causes light scattering.
It can also cause part swelling or aesthetic defects.
Process Control
Venting must be checked to prevent this issue. Increasing the holding pressure helps collapse the voids.