Meaning
Viscous energy losses occur when a polymer melt flows from a wider reservoir into a narrower die or gate during extrusion or molding. The resulting entry pressure drop represents the pressure required to force the polymer chains to accelerate and align as they enter the restricted flow channel. High values indicate strong resistance to rapid deformation.
Flow Resistance
Shear rates increase dramatically as the melt approaches the restriction. This rapid transition forces the polymer chains to stretch along the flow direction, generating high extensional stress. Rheologists measure this parameter using capillary rheometry to assess the processing behavior of resins under industrial conditions.
Melt Behaviour
Molecular weight distribution affects the magnitude of the pressure change at the contraction point. Highly branched polymers exhibit greater extensional viscosity and consequently yield a larger entry pressure drop than linear polymers of similar molecular weight. Part manufacturers monitor this pressure value because it determines the total injection force required to fill a cavity.
Low extensional viscosity minimizes the pressure required, which reduces energy consumption and limits the wear on molding machinery.
Processing Impact
Excessive pressure gradients at the channel entrance can trigger flow instabilities. This physical stress often leads to melt fracture, which causes surface roughness and structural defects in extruded profiles. Careful gate design and optimized process temperatures can mitigate these defects.