Meaning
Chemical exchange reactions occurring between ester linkages and hydroxyl or acid end groups alter the macromolecular architecture of polyester blends at elevated temperatures. Transesterification degradation governs molecular weight distribution changes, random copolymer formation and loss of mechanical integrity during the melt processing of condensation polymers. The reaction path operates primarily across polyester and polycarbonate families during melt extrusion, compounding and injection moulding stages.
Chemical exchange ceases once temperatures drop below polymer crystallization points or when functional chain ends are chemically blocked.
Melt Chemistry
Ester interchange reactions proceed via nucleophilic attack of hydroxyl or carboxyl terminal groups on adjacent ester carbonyl carbons within the molten matrix. In condensation polymers like polybutylene terephthalate and polyethylene terephthalate, transesterification can cause both chain cleavage and transesterification scrambling. Residual polymerization catalysts, such as titanium, antimony or zinc complexes, accelerate these exchange rates at standard processing temperatures.
The reaction alters blocky chain sequences, converting structured multi-phase blends into random, single-phase copolymers. Unchecked interchange leads to polydispersity shifts, rapid melt viscosity drops and progressive embrittlement.
Moisture Interaction
Processing polyesters in the presence of trace water triggers hydrolytic scission that amplifies transesterification rates. Water cleaves ester bonds into shorter chains with active hydroxyl and carboxylic acid ends, multiplying the reactive sites that drive transesterification loops. The resulting loss of molecular weight causes sudden drops in zero-shear melt viscosity inside the injection barrel.
Extrusion operations experience surging, drooling and unstable bubble formation due to this rapid loss of melt strength. Strict dehumidifying drying prior to processing is mandatory to keep moisture levels below 0.02 percent.
Performance Consequences
Changes in chain structure caused by transesterification disrupt regular chain packing, lowering both the melting point and the crystallization rate. Parts moulded from degraded resin exhibit lower heat deflection temperatures, higher post-mould shrinkage and severe loss of notched izod impact strength. Regrind additions compound these defects by re-introducing active catalyst residues and degraded chains into virgin material batches.
Specialized additives, such as organophosphites, are dry-blended into resin feeds to coordinate with residual catalysts and suppress transesterification pathways. Controlling residence times and melt temperatures preserves polyester chain structures to prevent functional component failures.