Meaning
Thermal solidification of the outer boundary layer occurs when polymer melt contacts a cold mould surface before the cavity fills completely. Skin freezing establishes a high viscosity barrier that effectively narrows the flow channel for the remaining molten plastic. High gate pressure becomes necessary to force material through this restricted passage during the packing stage.
Excessive cooling of the surface creates an insulating layer that prevents proper pressure transmission to the distal reaches of the part.
Moulding Physics
Cooling rates dictate the thickness of the frozen layer along the core and cavity walls. Faster cycle times or lower mould temperatures increase the depth of this solidified crust relative to the molten core. Polymer chemistry influences the window of operation because semi-crystalline resins develop a more defined transition zone than amorphous plastics.
Thin wall sections suffer from premature flow stoppage when the freezing rate exceeds the injection speed. Tooling geometry determines the ratio of surface area to volume, which governs how quickly the part solidifies during the filling phase.
Defect Correlation
Short shots happen when the flow front reaches a total blockage before the cavity reaches its intended volume. Sink marks appear when the frozen skin lacks the structural integrity to support the shrinkage of the interior molten mass as it cools. Surface defects like hesitation marks indicate local variations in the thickness of the solidified layer caused by flow front turbulence.
Internal voids manifest when the core remains fluid while the peripheral skin seals off the feed source. Dimensional instability follows when the thickness of the skin varies across the surface area of a single moulded component.
Economic Impact
Regrind usage changes the viscosity of the material, which alters the balance of the freezing layer and requires updated injection parameters. Virgin resin batches with narrow molecular weight distributions show more predictable solidification profiles than recycled stocks. Tool maintenance costs rise when operators increase injection pressure to compensate for restrictive skin formation.
Longer cycle times allow for more complete packing but reduce the total output of a production line per hour. Material waste rates correlate directly with the frequency of incomplete fills caused by improper thermal management of the mould surface.