Meaning
High-temperature degradation of polyester resins occurs when water molecules react with ester linkages at elevated processing temperatures. Rapid polyethylene terephthalate hydrolysis breaks long polymer chains into shorter fragments, lowering molecular weight and reducing melt viscosity during extrusion or injection moulding. The chemical reaction ceases when residual moisture drops below critical reaction thresholds prior to plasticating the resin.
Chain Cleavage
Heat and water act synergistically to cleave the ester bonds in the polyester backbone, producing carboxylic acid and hydroxyl end groups. Free carboxylic acid end groups catalyze further chain scission, accelerating reaction rates inside the melt stream. Processing un-dried PET flake increases polyethylene terephthalate hydrolysis, resulting in severe loss of intrinsic viscosity and brittle mechanical behavior in molded preforms.
Solid-state polymerization can reverse chain cleavage by reforming ester linkages under high vacuum and elevated temperatures.
Viscosity Loss
Lower molecular weight reduces the melt strength of PET, causing wall thickness variation in stretch blow molded bottles and melt sagging during profile extrusion. Dropping intrinsic viscosity below design limits causes preforms to crack during blowing operations.
Moisture Limit
Pre-drying virgin or recycled polyester resin to a moisture content below fifty parts per million prevents ester bond cleavage during melt processing. Maintaining strict moisture limits protects mechanical performance across long production runs.