Meaning
Quantitative measure of water content in polymer pellets before melt processing is expressed as a ratio of water mass to total resin mass to prevent thermal degradation during conversion. Monitoring parts per million moisture enables injection moulders to verify that hygroscopic resins have been dried to safe levels before injection. This process metric governs the success of the melting step and prevents hydrolysis from breaking the polymer chains.
The requirement is not critical for non-hygroscopic resins like polyethylene.
Moisture Measurement
Moisture content is measured using Karl Fischer titration or automated loss-on-drying instruments designed for engineering plastics. The analysis requires a sealed sample taken directly from the dryer hopper to avoid absorption of moisture from the ambient air. This test provides a precise numerical value.
It ensures the moulding process runs within safe limits.
Process Consequence
If the moisture level exceeds eighty parts per million for polycarbonate, the polymer undergoes rapid hydrolysis during melting, causing a drop in molecular weight and catastrophic brittleness. The molded parts will fail under low impact forces, and the scrap rate will increase. Furthermore, high moisture causes splay marks on the surface of the parts, which ruins their appearance.
These defects can be avoided by checking the moisture level before every production run.
Sourcing Rule
Incoming resin bags must be kept sealed in dry storage to prevent moisture pick-up, especially in humid moulding shops. When sourcing recycled regrind, the moisture variations can be extreme, demanding adaptive drying protocols to ensure consistent processing. If the material is sourced with high moisture, the drying time must be extended, which increases energy consumption and delays the production schedule.
Setting clear moisture limits in the purchasing specification helps moulders hold suppliers to a high standard and prevents process instability.