Meaning
Kinetic force exerted by molten polymer against the internal surfaces of a mould during the injection phase. This cavity filling pressure determines how well the resin replicates the tool surface and overcomes the flow resistance of the geometry. It terminates when the cavity reaches volumetric capacity and the machine switches to holding pressure.
Melt Resistance
Peak resistance measured at the nozzle or via internal sensors indicates the energy required to move the melt front. While the machine hydraulic pressure is often the recorded value, the actual cavity filling pressure is lower due to pressure drops across the runner and gate. A high viscosity material like polycarbonate requires more force than a low viscosity polyolefin.
This value fluctuates if the melt temperature drops or if the material contains a higher ratio of regrind than the virgin specification allows.
Defect Consequence
Insufficient force leads to incomplete parts or a poor surface finish where the melt fails to pack against the grain of the steel. Excessive cavity filling pressure causes the mould halves to deflect or blow open, resulting in material leaking across the parting line. Flash becomes more likely if the clamping force cannot counteract this internal expansion.
Measurement Distinction
Realized values differ from theoretical calculations found on a material datasheet. A moulder observes that thin walls or long flow paths increase the required effort compared to thick walled parts. The sensor data provides a window into the consistency of the resin batch.