Meaning
Rapid heating of the mould cavity surface during the injection phase followed by rapid cooling before ejection allows the production of parts with high gloss finishes and no visible weld lines. Implementing variothermal tooling is highly effective when processing amorphous polymers with high glass transition temperatures or materials with high filler content. This dynamic temperature control prevents the polymer from freezing prematurely on the mould wall, which ensures excellent replication of the cavity surface texture.
Temperature Cycling
Alternating between high-temperature steam and cold water within the tool’s cooling channels drives the surface temperature of the cavity up and down during each cycle. In variothermal tooling, this active thermal cycling must be closely coordinated with the injection moulding machine’s cycle. The cavity surface is heated to a temperature above the polymer’s glass transition temperature before injection starts, and is then cooled rapidly to solidify the part for ejection.
Surface Improvement
Elimination of cosmetic defects such as weld lines, sink marks, and fiber-readout is the primary objective of this dynamic temperature control method. When variothermal tooling is used, the polymer melt remains fluid longer at the cavity surface, which allows the material to blend completely at weld lines and eliminates the microscopic V-notch that causes mechanical weakness. This fluid state also prevents glass fibers in reinforced resins from rising to the surface, resulting in a smooth finish even with highly filled materials.
Cycle Penalty
Longer cycle times are a direct consequence of the time required to heat and cool the steel mould during each shot. This cycle penalty must be balanced against the benefit of eliminating secondary operations like painting or coating to achieve the desired surface finish.