Meaning
Sudden or progressive loss of functionality in an injection mould prevents the production of parts that meet the required specifications. Tool failure occurs when the steel components can no longer withstand the mechanical loads or thermal stresses of the moulding cycle. This condition ranges from small cosmetic cracks to catastrophic fractures of the main plates or cavities.
It is the primary cause of unplanned production stops in high-precision moulding.
Fracture Mechanism
Excessive injection pressure or poorly supported inserts cause the metal to deform or snap under load. Stress concentrations at sharp corners or thin walls are often the starting point for a crack that propagates through the core. If the clamp force exceeds the strength of the tool, the parting lines may crush and lead to permanent flash.
High-hardness steels are particularly susceptible to brittle fracture if they are not tempered correctly.
Thermal Fatigue
Repeated cycling between the melt temperature and the cooling water temperature creates internal expansion and contraction cycles. This heat checking on the surface of the cavity leaves visible lines on the plastic parts. Over thousands of shots, these small defects deepen and can eventually compromise the integrity of the cooling channels.
Remediation Path
Evaluation of the damage determines if a repair is possible through laser welding or if a new component must be machined. Extensive failures often indicate a flaw in the original design or the selection of an inappropriate steel grade. Analyzing the root cause prevents the same issue from recurring.