Meaning
Layer of oriented polymer chains at the surface of a moulded part exhibits different refractive properties than the bulk material due to high shear during injection. The formation of a strain birefringence optical skin occurs as the melt freezes instantly upon contact with the cold tool wall. This localized stress alters the polarization of light passing through the component, creating visible patterns or measuring errors.
Surface Stress
High velocity flow through the gate causes the molecules near the wall to stretch and align in the direction of the melt front. Because this alignment is frozen in place, the strain birefringence optical skin remains a permanent feature of the part.
Optical Distortion
Transmission of polarized light reveals rainbow like fringes where the internal stresses are highest. For precision lenses or displays, a heavy strain birefringence optical skin is a major defect that ruins the optical performance. These stresses can also lead to warping or environmental stress cracking over time.
Process Control
Increasing the mould temperature or reducing the injection speed helps to relax the molecular orientation before the resin solidifies. A thicker strain birefringence optical skin is often the result of low melt temperatures or excessive packing pressure. Monitoring these variables is the primary way to ensure the optical clarity of the final product.
Frozen molecular stress directly impacts the refractive index uniformity of the part.