Meaning
Visual surface defect characterized by metallic or pearlescent lines following the direction of the melt flow suggests the presence of gas. Trapped bubbles against the mold wall during injection result in the appearance of silver streak splay. This defect usually requires immediate adjustments to the drying or processing settings.
Moisture Presence
Pellet moisture levels must be reduced through desiccant drying before the material enters the barrel. Water trapped in the resin vaporizes into steam that creates silver streak splay as the bubbles stretch out in the mold cavity. Because the defect is often caused by inadequate drying, checking the dew point of the dryer becomes the first step in troubleshooting the problem.
Proper drying eliminates the source of the gas and prevents the streaks from forming on the part surface.
Melt Turbulence
Air trapped in the melt stream can also create these streaks if the injection speed is too high. Rapid flow creates turbulence that prevents silver streak splay from being absorbed or vented properly. Slowing the injection rate or increasing the back pressure can help force the gas out of the melt.
Aesthetic Failure
Streaks on the part surface make the component unsuitable for consumer facing applications. Because silver streak splay is a visual inconsistency, it usually leads to the rejection of the entire batch. Consistent processing conditions and dry material are necessary to prevent the recurrence of this defect.