Meaning
Decomposition of unstable oxygen-oxygen bonds in pre-oxidized polymer chains leads to the generation of highly reactive alkoxy and hydroxy radicals. This reaction step of secondary hydroperoxide cleavage occurs at elevated processing temperatures and initiates the rapid reduction of polymer chain lengths. The process represents a major phase in autoxidation.
Reaction Pathway
Thermally induced dissociation of the hydroperoxide group yields a highly reactive alkoxy radical and a hydroxyl radical. The occurrence of secondary hydroperoxide cleavage accelerates the degradation because each initiating event generates two new free radicals. These newly formed radicals then abstract hydrogen from neighboring chains to continue the cycle.
Defect Generation
The creation of volatile by-products like ketones and alcohols during this process causes physical defects in the molded parts. When secondary hydroperoxide cleavage is active, these low molecular weight species volatilize and form microscopic gas bubbles in the molten polymer. This gas leads to splay marks on the surface of the injection-molded components.
Additionally, the decrease in average molecular weight reduces the impact strength. Processors observe a marked increase in melt flow rate when this reaction is unchecked.
Stabilization Target
Preventing this cascade requires the inclusion of secondary antioxidants like phosphites or thioesters in the compounding stage. These additives destroy the hydroperoxides before secondary hydroperoxide cleavage can take place. Effective stabilization preserves the physical properties of the recycled resin.