Meaning
Fluid turbulence within the cavity results from an excessive injection velocity that forces the polymer stream into a distinct narrow path rather than filling the area in a uniform front. When jetting occurs, the high-speed material shoots across the mold surface before the gate can build adequate pressure to pack the remainder of the tool. This phenomenon creates an internal structural discontinuity which weakens the mechanical integrity of the finished part.
Residual surface marks often appear as snaking patterns or serpentine ripples along the flow path.
Melt Mechanics
High injection speeds during the initial filling phase drive this behavior by exceeding the critical velocity where laminar flow transitions into uncontrolled chaotic dispersion. The viscosity profile of the resin influences how readily the material deviates from a stable front, as lower viscosity polymers demonstrate a higher susceptibility to such instability. Engineers adjust the injection speed profile during the first stage of the cycle to mitigate these conditions.
Precise gate geometry also acts as a primary control factor by redirecting the melt against a wall to dissipate kinetic energy before it enters the main cavity volume.
Production Penalty
Surface defects caused by this flow condition force the immediate rejection of affected components during quality inspection. Internal voids that accompany these ripples compromise the load-bearing capacity of the part, which leads to failure under stress in applications requiring structural uniformity. Regrind usage complicates the situation because material consistency shifts relative to virgin resin, causing unexpected changes in local viscosity that demand frequent adjustments to the machine setpoints.
Thermal Variance
Localized cooling occurs prematurely along the path of the stream as the material loses heat to the tool surface before the cavity fills entirely. This rapid chilling creates a solidified skin that prevents the subsequent bulk material from bonding correctly with the surrounding structure. Moulders observe that the resulting thermal gradient across the part dimensions causes warpage even after the mold successfully achieves full volume.
Proper gate placement ensures the stream impacts a perpendicular face and prevents the formation of these weak knit lines across the final geometry.