Meaning
Tensile forces act on a polymer melt when it undergoes rapid acceleration or narrowing through a die or gate. This extensional flow stress differs from shear stress because it involves the stretching of polymer chains along the direction of travel. High molecular weight resins exhibit strong resistance to this deformation, a property often described as melt strength.
It governs how the material behaves in processes like blow moulding or film stretching where the melt is unsupported.
Molecular Orientation
Rapid changes in the cross-sectional area of a flow channel force the coiled polymer molecules to straighten. As extensional flow stress increases, the degree of molecular alignment in the final part becomes more pronounced. This orientation improves the tensile strength of the part in one direction but creates potential weak points in the transverse direction.
Regrind materials often show lower resistance to stretching due to the thermal degradation of long chains during previous heat cycles.
Defect Origin
Sudden contraction in a runner system leads to localized energy buildup that can cause physical rupture of the melt. When extensional flow stress exceeds the cohesive strength of the resin, defects such as melt fracture or sharkskin appear on the surface. These irregularities ruin the aesthetic finish and can introduce stress concentrators that lead to premature part failure.
Correcting these issues usually requires a redesign of the gate transition or a reduction in injection speed. Internal stresses trapped during this phase may also lead to part warpage once the material cools and crystallizes. If the pressure drop across a gate is too high, the resulting stretch can pull the polymer apart at a microscopic level.
Processing Limit
Operating windows for extrusion and injection are often constrained by the elasticity of the polymer. The extensional flow stress determines the maximum drawdown ratio possible before the film or parison snaps. Datasheet values for shear viscosity do not always predict this behavior, making extensional testing necessary for high-performance resins.
Production rates stay low when the material cannot withstand the forces of rapid acceleration through the tooling.