Meaning
Solidification kinetics occurring at the cold interface between a polymer melt and a mold surface govern the instantaneous cross-sectional flow area during cavity filling. Transient heat transfer models track frozen skin development as molten resin contacts cold tool steel and immediately freezes into a stationary boundary layer. The thickness of this solid layer grows over time as heat transfers into the mold wall, restricting the core channel where hot polymer continues to flow.
Moulders balance melt temperature and injection velocity to control skin growth and prevent premature gate freeze-off.
Shear Layering
High velocity gradients between stationary frozen walls and flowing central melt create severe shear stress concentrations along the phase boundary. High shear rates during frozen skin development orient polymer chains along the flow direction, producing anisotropic mechanical properties across the part wall.
Flow Restriction
Rapid cooling thickens the stationary outer layer, forcing remaining liquid resin through a progressively narrower central flow channel. Uncontrolled frozen skin development increases injection pressure requirements, potentially causing incomplete filling in thin sections.
Sink Mitigation
Internal volume shrinkage during polymer cooling pulls surface material inward when the outer skin remains hot and pliable. Achieving rapid frozen skin development forms a rigid outer shell that resists surface sink marks, forcing volumetric shrinkage into internal micro-voids instead.