Meaning
Tooling failure mechanism in which asymmetrical melt front pressure causes an unsupported metal core pin to bend or shear off inside an injection mould cavity. High polymer viscosity during the fill phase exerts lateral forces against slender mould inserts. Tool steel selection and gating location dictate the maximum stress a pin withstands before plastic deformation occurs.
The phenomenon applies to thin-walled technical mouldings containing narrow internal lumens or fastener holes.
Imbalance Velocity
Unbalanced filling channels generate uneven lateral force vectors across opposing faces of internal core inserts. Imbalanced gate placement drives polymer melt along one side of a pin prior to complete cavity filling. Core pin shearing occurs when differential pressure exceeds the yield strength of the hardened tool steel insert during high-speed injection.
Lowering injection velocity reduces peak melt pressure but risks premature freezing in thin wall sections.
Pin Deflection
Bending moments generated by plastic flow alter part dimensions before structural yield occurs. Deflection of slender pins alters hole concentricity and produces wall thickness variations across the moulded component. Core pin shearing represents the ultimate mechanical failure resulting from unchecked deflection under melt flow stress.
Steel Selection
Material selection for slender mould inserts balances toughness against wear resistance. Premium grades such as H13 or S7 tool steel undergo vacuum heat treatment to maximize shear strength while resisting thermal shock. Regrind resin containing abrasive fillers accelerates pin wear, compounding the risk of mechanical bending under pressure.
Maintaining balanced gating layouts protects core inserts during continuous production cycles.