Meaning
Solid-to-gas transition describes the phase change where a solid chemical compound converts directly into a vapor without passing through a liquid state under specific thermal and pressure conditions. During injection moulding of polycarbonate resins, bisphenol-a sublimation occurs when residual monomer molecules migrate to the surface of the melt and vaporize upon exiting the nozzle. This vapor then deposits onto cooler mould surfaces as a white crystalline residue, which deteriorates the surface finish of subsequent moulded parts.
In medical and food-contact applications, this phenomenon is critical because the presence of free monomer on the component surface can trigger regulatory non-compliance.
Phase Transition
Elevated melt temperature accelerates the rate at which residual monomer escapes from the polymer matrix. High-vacuum venting in the extruder barrel during compounding represents the primary method for reducing residual monomer levels before the material reaches the moulding floor. When compounding is insufficient, bisphenol-a sublimation becomes highly pronounced during the high-temperature phases of the moulding cycle.
Process Impact
Deposition of the crystalline monomer on polished mould cavities creates a physical barrier that prevents replication of the high-gloss finish. Tooling must be cleaned frequently to prevent the transfer of these deposits to the moulded parts, which increases production downtime and scrap rates. In optical lens production, this build-up causes surface scattering and rejects.
Defect Prevention
Reduction of the cylinder temperature profile represents the most direct method to curb the vaporization rate of the monomer during a run. Mould temperature control and venting design also assist by directing the outgassed vapor away from critical cavity areas before it can deposit. Maintaining a dry resin with less than 0.02 percent moisture minimizes hydrolytic degradation, which otherwise generates additional free monomer during processing.