Meaning
Temperature variations occurring between different cavities of a multi-cavity mould stem from the non-symmetric distribution of frictional heat within the runner system. This shear-induced imbalance appears when melt flows through a tee-junction and the high-shear material near the walls is diverted to one side of the split while the cooler core material goes to the other. High-cavitation tools often produce parts with different dimensions or weights despite having identical steel dimensions in every cavity.
Melt Distribution
Rheological properties of the polymer influence how heat builds up during the high-speed injection phase. In a standard H-pattern runner, the shear-induced imbalance causes the inner cavities to receive hotter, less viscous melt than the outer cavities. This difference leads to uneven packing and varied cooling rates across the set of parts.
Defect Analysis
Variations in part weight or flash formation usually indicate that the thermal profile of the melt is not uniform at the gate. If one cavity fills faster than another, the cause is often the thermal history of the material rather than a physical blockage. Adjusting the melt temperature at the barrel rarely solves this issue because the heat is generated by the flow velocity within the runner itself.
Tool Correction
Engineering solutions to this problem involve the use of specialized runner inserts that rotate the melt stream to redistribute the heat. These melt flippers or stratified flow mixers ensure that every cavity receives a representative mix of high-shear and low-shear material. Implementation of these components reduces the scrap rate by narrowing the statistical distribution of part properties across the run.