Meaning
Shredded, washed, and size-reduced particles of rigid or flexible post-consumer and post-industrial plastics form intermediate raw material feedstocks for compounding and direct extrusion. Recyclers generate polyolefin flakes from discarded polyethylene bottles, polypropylene crates, and industrial film waste through mechanical shredding and sink-float density separation. The material format bridges recovered whole articles and pelletised secondary resins, with its application ceiling defined by bulk density deficits that prevent stable feed rates into standard single-screw injection moulding barrels.
Size Morphology
Mechanical granulators reduce sorted hollowware and films into jagged planar particulates ranging from two to twelve millimetres in dimension. Sourcing polyolefin flakes requires rigorous density sorting to separate polypropylene from high-density polyethylene, because cross-contamination creates immiscible phases that cause brittle part failure. Bulk density remains low, ranging between two hundred and three hundred grams per litre, necessitating force-feeders or crammer hoppers on primary extrusion machinery.
Fines smaller than two millimetres cause bridging in gravimetric blenders, complicating precise additive dosing.
Conversion Route
Direct processing of washed flake into finished structural goods bypasses the thermal history of an intermediate pelletisation step. Compounding polyolefin flakes requires twin-screw extruders equipped with high vacuum degassing to extract residual moisture, volatile detergent residues, and low-molecular-weight contaminants. Incorporating functional coupling agents and virgin resin balances the physical drop caused by accumulated thermal histories.
Without adequate melt filtration, un-melted foreign plastics cause pinholes in blown film or burst thin-wall injection parts.
Economic Value
Procuring clean un-pelletised flake offers significant raw material cost discounts compared to certified post-consumer recycled pellets. Variations in melt flow index, contamination by incompatible polymers, and inconsistent colour across flake lots introduce operational instability. Moulding directly from flake demands continuous process monitoring, as inconsistent bulk density induces screw recovery time drift.
Processors balance low procurement costs against the wear on feeding equipment caused by residual abrasive dirt on flake surfaces.