Meaning
Internal stress reduction occurs in amorphous thermoplastics as the molecular chains reorganize toward an equilibrium state. The polycarbonate relaxation process typically follows the high pressure injection stage where chains are forced into an unnatural orientation. If this stress is not managed, the part may later crack or warp when exposed to chemicals or heat.
Dimensional Change
Physical movement of the part geometry is a direct result of these internal shifts. As polycarbonate relaxation takes place, the external dimensions of a lens or housing may shrink slightly over several days. Precision optics require a stable environment and sometimes an annealing step to ensure that the focal length and surface profile remain within the tight tolerances required by the design.
Thermal Influence
Temperature levels during storage and use determine the speed at which molecules move. Higher ambient temperatures accelerate polycarbonate relaxation, causing the material to reach a stable state more quickly. Moulders often use heated tools to reduce the initial frozen-in stress, which minimizes the amount of relaxation that happens after the part leaves the factory.
Moulding Variable
Processing parameters such as pack pressure and cooling time directly affect the level of residual tension. Controlling polycarbonate relaxation requires a balance between rapid cycle times and the need for a stress free part. Monitoring helps.