Meaning
Spectroscopic absorbance ratios comparing degraded carbonyl bonds to stable carbon skeleton vibrations determine the extent of oxidative breakdown across a plastic specimen. In quality control and post-consumer polyolefin reprocessing, the oxidation index quantifies thermal, mechanical and photo-oxidative aging experienced by resins during prior life cycles or aggressive processing. The value governs polymer stability assessments, incoming scrap classification and stabilization additive dosing for recycled feedstocks.
It stops applying to intrinsically oxygenated polymers, such as polyesters, polyamides or polycarbonates, where carbonyl groups form fundamental repeating links in the virgin backbone chain.
Infrared Calculation Route
Laboratories measure the index by collecting transmission or attenuated total reflectance spectra across thin film specimens using Fourier transform infrared spectrometers. The technician measures the baseline-corrected peak height or area of the carbonyl band centred near seventeen hundred and twenty reciprocal centimetres, which represents aldehydes, ketones and carboxylic acids. This value is divided by the absorbance of a reference band unaffected by processing degradation, such as the carbon-hydrogen scissor vibration at fourteen hundred and sixty reciprocal centimetres in polyethylene.
Dividing by this unvarying internal standard neutralizes variations in specimen thickness, contact angle and optical scattering. A higher calculated ratio signifies deeper degradation through radical chain branching and hydroperoxide breakdown.
Degradation Pathway Consequence
Polyolefins exposed to elevated barrel temperatures, high shear fields or prolonged outdoor radiation develop free radicals that react rapidly with oxygen. These peroxy radicals extract hydrogen atoms from neighbouring polymer backbones, generating unstable hydroperoxides that split into reactive alkoxy and hydroxy species. The subsequent beta-scission reactions cleave polymer chains, depressing melt strength, while radical recombination leads to uncontrolled crosslinking.
In polyethylene, elevated oxidation values correlate with crosslinking, visible gel clusters and falling melt flow rates. In polypropylene, chain cleavage dominates, driving the melt flow index sharply upward, making the material brittle and unsuited for structural moulding.
Injection Processing Hazard
Reclaimed resins delivered with high baseline oxidation values cause erratic flow fluctuations and structural failure in downstream processing tools. As oxidized pellets enter the feed throat, degraded functional groups cause inconsistent shear heating, which destabilizes cushion formation during the injection phase. Moulded articles exhibit embrittlement, low izod impact strength and premature stress cracking under minimal load.
Processors counteract oxidized scrap by blending it with prime virgin resin and feeding active primary hindered phenols coupled with secondary phosphite stabilizers during compounding. If the oxidation index climbs beyond established threshold limits, the resin is deemed unrecoverable for injection parts and routed down to thick-profile non-structural extrusion.