Meaning
Duration of polymer exposure to elevated temperatures within the barrel defines the thermal history of the material during processing. The calculation of melt residence time governs the stability of the molecular chains from the moment the resin melts until it exits the nozzle. It does not apply to the solid conveying zone where temperatures remain below the transition point or to post mold cooling where the polymer has already solidified.
Thermal Exposure
Longer cycles increase the cumulative heat absorbed by the polymer melt. Each resin possesses a specific limit beyond which the polymer begins to break down. When the screw remains stationary during long cooling times, the material in the transition zone degrades rapidly.
Degradation Consequence
Chemical degradation of the polymer chains alters both the mechanical properties and the appearance of the molded part. Severely degraded resin exhibits lower tensile strength and visible discoloration. The drop in viscosity can also cause flashing at the parting line.
Molding Adjustment
Minimizing the barrel temperature or reducing the shot to barrel ratio lowers the duration of heat exposure. If a mold runs on a press with an oversized barrel, the operator must adjust the process parameters to maintain material integrity. Purging with a stable resin during interruptions prevents degradation.