Meaning
Flow instabilities arising at critical shear stress boundaries during die extrusion lead to surface distortions on extruded polymer profiles. Reaching the threshold of melt fracture initiation converts smooth extrudate surfaces into rough, wavy, or sharkskin textures as resin leaves the die orifice. High molecular weight polymers with narrow molecular weight distributions display strong susceptibility to flow instabilities at lower extrusion speeds.
Surface roughness damages optical clarity, dimensional tolerances, and sealing performance in film and tubing products. Fluoropolymer processing aids added to linear low-density polyethylene delay flow instability onset by reducing wall shear stress at the metal boundary.
Critical Stress
Wall shear stress in the die land exceeding two hundred kilopascals initiates periodic stick-slip motion between the melt and the metal wall. Rapid acceleration of the outer melt layer upon exiting the die exit creates localized tensile stresses that rupture the polymer skin. Increasing melt temperature reduces shear stress, delaying surface distortion without changing die geometry.
Extrusion throughput limits depend directly on this critical stress boundary.
Surface Distortion
Extrudate appearance degrades from mild loss of gloss to severe sharkskin patterning as wall shear rates increase. Highly unstable flow produces gross melt fracture, forming distorted helical extrudates that ruin product dimensions. Defective tubing and film profiles fail quality specifications, forcing line speed reductions.
Additive Mitigation
Fluoropolymer processing additives coat the interior die surface to promote slip at the wall. The dynamic slip layer reduces local shear stress below the instability threshold, allowing higher production rates. Processing additives permit high-throughput processing of tough linear polyolefins without surface defects.