Meaning
Remaining volume of polymer in front of the injection screw at the end of the holding phase ensures that pressure is continuously applied to the cooling part. Maintaining a melt cushion prevents the screw from bottoming out against the barrel head. If the screw reaches the end of its stroke before the holding time is complete, the machine can no longer transfer packing pressure to the resin in the cavity.
This results in poor part compaction and high weight variation. This remaining material acts as a physical buffer that transmits the hydraulic force of the screw directly to the runner system.
Process Monitoring
Monitoring the size of this residual volume provides a quick assessment of process stability from shot to shot. If the melt cushion fluctuates or drops to zero, it often indicates a leaking check ring or inconsistent melt density. A worn check ring allows material to slip backward over the screw during injection, which reduces the effective hold pressure.
Moulders track this value to detect mechanical wear before it causes major part defects.
Sizing Criteria
Recommended sizes for this buffer zone are typically between three and six millimeters of screw stroke. Having too large a melt cushion increases the residence time of the polymer in the heated barrel. This can lead to thermal degradation of sensitive resins, resulting in cosmetic streaks or lost physical properties.
Setting the cushion to a minimal but stable volume ensures both high process repeatability and material integrity.
Recovery Phase
Plastification of the next charge of resin occurs immediately after the holding phase ends. The screw rotates and moves backward, preparing the next dose while leaving the cushion in place.