Meaning
Standard test methods for measuring the flow behavior of dilute polymer solutions determine the molecular weight and polymer chain extension of soluble resins. The procedure defined by intrinsic viscosity ASTM D2857 establishes the baseline for assessing thermoplastic degradation caused by processing or environmental exposure. This standard provides a reproducible metric for comparing the molecular structure of different polymer batches.
Testing Protocol
Capillary viscometers measure the efflux times of both the pure solvent and the polymer solution at a controlled temperature. Applying the formulas of intrinsic viscosity ASTM D2857 requires several dilute concentrations to extrapolate the viscosity to zero concentration. This extrapolation removes the effects of intermolecular interactions and isolates the contribution of individual polymer chains to the flow resistance.
Moulding Relationship
Moulders of polyethylene terephthalate preforms rely on this test to ensure the incoming resin has sufficient melt strength. A decrease in the intrinsic viscosity indicates that hydrolysis or thermal degradation has broken the polymer chains during compounding or drying. When the values fall below the specified limit, the extruded preforms fail during the blow moulding step due to localized wall thinning.
Process Impact
Processing regrind material typically reduces the average length of the polymer molecules and decreases the measured viscosity value. This degradation forces the moulder to adjust the injection speed and melt temperature to compensate for the easier flow and lower viscosity of the degraded polymer. Inconsistent viscosity across runs results in flash at the parting line or incomplete filling of the mould cavities.
Maintaining a constant ratio of virgin resin to regrind is therefore necessary to stabilize the process. By controlling the feed composition, the operator preserves the mechanical properties of the moulded part.