Meaning
Condensable chemical fractions that outgas from polymer matrices at elevated operational temperatures collect on nearby surfaces as semi-volatile films or oily deposits. Automotive interior standards and optical enclosure specifications identify fog as the gravimetric or photometric deposit generated when a moulded part undergoes thermal stress under sealed test conditions. The measurement governs plasticizers, antioxidants, low molecular weight oligomers and process waxes capable of evaporating between sixty and one hundred and thirty degrees Celsius.
It stops applying to ambient volatile organic compounds that remain in the gas phase and do not settle onto cold glass substrates.
Test Chamber Method
Standardized chamber runs measure these emissions using either gravimetric collection or optical reflectometry following methods such as DIN 75201 or ISO 6452. A prepared specimen rests at the bottom of a heated beaker covered by a cooled glass plate held at sixteen to twenty-one degrees Celsius. For the gravimetric method, designated as method G, the laboratory measures tare and final weights of aluminium foil discs that capture the condensate over sixteen hours at one hundred and twenty degrees Celsius.
The photometric route, method F, measures light reflectance off the fouled glass surface after three hours at one hundred degrees Celsius, expressing the result as a percentage of initial surface reflectivity. Photometric yield decreases sharply when aliphatic lubricants and aromatic plasticizers form droplets on the chilled lens.
Tooling Fouling Consequence
Moulding polymers loaded with unstable additive packages precipitates continuous maintenance penalties on the production floor. Semi-volatile components that volatilize during the plasticizing stage migrate toward the mould vents, leaving waxy varnishes across core details, optical lenses and textured cavity faces. Gas venting channels gradually clog, causing localized burn marks, diesel effect scorches and short shots in high-volume runner systems.
Technicians must cycle the press down to wipe tool faces with solvent, interrupting cycle continuity and degrading automated manufacturing yields. Lower-fog resins, produced using high-molecular-weight Hindered Amine Light Stabilizers and secondary phosphites, extend intervals between tool strippings by three to five production days.
Specification Control
Automotive converters establish strict fog limits on polypropylene, polyamide and elastomer compounds intended for passenger cabin components. Virgin compounders meet these thresholds by using reactive extrusion stripping to remove residual dimer fragments, alongside synthetic ester lubricants instead of low-cost oleamides or erucamides. Recycled compounds struggle to maintain compliant values because unwashed cleaning residues and migrating plasticizers from post-consumer inputs contaminate the base melt.
Incoming quality checks reject lots yielding photometric scores under eighty percent or gravimetric condensates exceeding two milligrams per part surface area. Controlling supplier formulations prevents premature windshield hazing and dashboard degradation in commercial vehicles.