Meaning
Surface wave patterns on injection moulded plastic parts represent visual imperfections caused by unstable advancement of the melt front inside the mold cavity. These surface ripples occur when the advancing polymer skin freezes prematurely against the cold cavity wall and then rolls over under fluctuating velocity or pressure. The defect compromises cosmetic appearance without altering bulk tensile strength.
Boundary: the phenomenon is restricted to thermoplastic moulding processes where a molten front fills a closed cavity, excluding continuous extrusion or blow moulding.
Surface Defect
Molded components display alternating light and dark bands across cosmetic surfaces adjacent to structural features or changing wall thicknesses. Hesitation during cavity filling allows the leading polymer edge to cool below its glass transition or crystallization temperature before complete pack pressure arrives. The frozen skin buckles under subsequent pressure surges, creating visible gloss variations.
Regrind additions with varying melt flow rates worsen surface consistency by creating non-uniform viscosity fronts during filling.
Process Rheology
Viscous flow behavior during injection determines front stability. Lowering melt temperature or decreasing injection speed increases shear viscosity, accentuating hesitation marks as the polymer navigates restricted channels.
Gate Design
Moulding gate geometry directly dictates flow velocity profiles at entry. Small gate cross-sections induce high shear heating, which temporarily lowers melt viscosity but causes severe velocity changes when expanding into thick wall sections. Widening gate dimensions stabilizes front movement and suppresses flow marks.
Correct positioning ensures continuous forward motion without structural interruptions.