Meaning
Internal resistance value derived from the energy lost during the tearing of a polymer sheet. elmendorf tear uses a pendulum to continue a rip that was initiated by a sharp blade. The result is a direct measurement of the work done in tearing the specimen through a fixed distance.
Tearing Force
Gravitational energy is converted into mechanical work as the arm swings through the film. Low values of elmendorf tear indicate that the polymer chains do not have enough entanglement to resist the split. The measurement is recorded in grams or millinewtons.
Tear Directionality
Blown films exhibit different resistance levels depending on the axis of the test. In most cases, the machine direction elmendorf tear is notably lower than the transverse direction result. This difference occurs because the molecules are pulled tight along the flow line.
Stretching the bubble in the transverse direction can help to equalize these two values.
Surface Defect
Integrity of the specimen edge is critical for a valid test result. If the initial slit is not clean, the elmendorf tear value will be inconsistent. Rough surfaces or gels in the film can act as stress risers that accelerate the failure.
Laboratory technicians must inspect the blade for sharpness to ensure the cut is precise.