Meaning
Force per unit area acting at the interface between a polymer part and the mould surface during removal. Calculations for ejection shear stress help engineers determine if the part will deform or tear when pins push against it. This value depends on the normal force exerted by the shrinking resin and the coefficient of friction between the plastic and the steel.
A moulder encounters high resistance when the material grips deep ribs or textured walls.
Resin Behavior
Thermal contraction creates the pressure that drives the resistance during the demoulding phase. If the ejection shear stress exceeds the yield strength of the polymer at that specific temperature, the part suffers from stress whitening or punch-through. Semi-crystalline resins often require higher ejection forces because their high shrinkage rates clamp more tightly onto internal cores.
Process Variable
Packing pressure determines how much material is forced into the cavity to compensate for cooling. Excessive packing increases the ejection shear stress by preventing the part from pulling away from the cavity walls easily. Moulders adjust holding time and pressure to achieve dimensional stability without sacrificing the ease of part release.
Surface Impact
Surface finish on the tool walls notably alters the mechanical load required for removal. Polished surfaces or specialized coatings reduce the ejection shear stress and prevent scuffing on the part exterior. When the load stays within safe limits, the cycle time remains consistent and the tool avoids premature wear from abrasive resins.