Meaning
A testing standard quantifies the energy required to cause plastic film to fail under the impact of a free-falling dart. The procedure defined by astm d1709 dart drop involves clamping a specimen and dropping a weighted hemispherical dart from a specified height. This test provides a direct measurement of the toughness of a film, which is a critical specification for packaging and liners.
Method Variation
Two different procedures, known as Method A and Method B, utilize different drop heights and dart diameters. Method A uses a drop height of 0.66 meters, while Method B uses 1.50 meters for stronger or thicker films. Technicians determine the weight at which 50 percent of the specimens fail, which is recorded as the astm d1709 dart drop value.
Extrusion Variable
Processing conditions during film extrusion, such as the blow-up ratio and die gap, affect the impact strength. High orientation in the machine direction can lead to lower dart values even if the resin itself is high quality. Film producers monitor this value to ensure that the combination of resin selection and extrusion settings provides enough protection for the packaged goods.
Quality Control
Reliable impact resistance prevents bags from bursting during filling or transport. A sudden drop in this measurement often signals a problem with the resin blend or a change in the cooling rate of the bubble. This specification is more relevant to actual performance than simple tensile testing.