Meaning
The breakdown of polymer chains caused by the combined effects of high temperature and intense mechanical shear during processing. This thermal shear degradation reduces the molecular weight of the polymer, which impairs the mechanical properties and surface finish of the moulded parts. It commonly occurs in restrictive areas of the mould like gates, runners, or thin sections.
Physical Mechanism
High shear rates generate internal friction within the flowing polymer melt, raising its temperature far beyond the barrel heater settings. This physical mechanism is particularly severe in highly viscous resins processed at excessive injection speeds. It leads to chain scission, where the long polymer molecules break into shorter fragments.
Moulding Defects
Visible symptoms of this degradation include splay marks, discoloration, and black specks on the surface of the finished part. Mechanical testing of affected parts reveals a drop in impact strength and elongation at break. In severe cases, the degraded plastic releases corrosive gases that can attack the mould steel and ruin the cavity finish.
Preventing these issues requires adjusting the gate geometry or lowering the injection velocity to reduce shear rates.
Process Control
Moulders must balance injection speed with melt temperature to avoid this degradation. Optimizing screw design and using generous gate sizes also helps minimize shear stress. This careful control ensures the resin retains its intended performance characteristics.