Meaning
Mechanical resistance measurements quantify the force required to pull apart a heat-sealed seam on a flexible plastic package. Evaluating seal strength is essential to ensure that pouches and bags maintain their containment integrity during shipping, handling, and storage. This property is determined using tensile testing equipment that pulls specimen strips at a constant speed until the seal fails.
Measurement Technique
Tensile testers grip the unsealed ends of a sealed strip and measure the force required to peel the seal open. The maximum load and the energy absorbed during the peel test define the seal strength of the material combination. Test protocols must specify the peel angle and sample width to generate reproducible data for quality assurance records.
Material Formulation
Coextruded films use specialized sealant layers made from ethylene-vinyl acetate or metallocene linear low-density polyethylene to optimize sealing characteristics. Since seal strength depends on the molecular entanglement of the polymer chains across the interface, the resin composition must allow rapid diffusion at the seal temperature. Adjusting the vinyl acetate content in the sealant layer alters the activation energy of seal formation and improves seal integrity.
Processing Defect
Insufficient sealing temperature or pressure in the packaging machine leads to weak seals that fail under low impact forces. If the sealing temperature is too high, the polymer melts excessively and squeezes out of the seal area, which reduces the local thickness and lowers the seal strength. Continuous monitoring of the sealing parameters allows packaging lines to avoid weak seals and prevent product contamination caused by leaks.