Meaning
Degradation pathways in hydrocarbon polymers involve self-sustaining chemical reactions triggered by heat, light, or oxygen. Polyolefin auto-oxidation leads to chain scission, cross-linking, and a reduction in mechanical properties such as impact strength and elongation at break. This process occurs during both melt processing and long-term outdoor exposure.
Stabilizers are added to the resin to interrupt these reactions and prolong the useful life of the part.
Reaction Mechanism
The degradation begins when thermal energy or shear stress breaks a carbon-hydrogen bond to create a free radical on the polymer backbone. In the presence of oxygen, polyolefin auto-oxidation continues through a series of propagation steps that generate hydroperoxides. These hydroperoxides are unstable and split to form more radicals, which accelerates the degradation process.
This chain reaction will continue until the radicals are neutralized by primary antioxidants.
Processing Impact
During extrusion and moulding, high melt temperatures and intense shear can accelerate these degradative reactions. When polyolefin auto-oxidation occurs in the extruder, it causes changes in melt flow index that disrupt the consistency of the moulding process. Unchecked oxidation leads to discoloration, odor generation, and a drop in the toughness of the finished parts.
Processors monitor melt behavior to ensure that the stabilization package is performing correctly.
Sourcing Evaluation
Recycled polyolefins often possess a history of prior thermal degradation and may have depleted antioxidant levels. Testing for polyolefin auto-oxidation sensitivity helps purchasers determine if a recycled lot requires booster packages of stabilizers before compounding.