Meaning
Low molecular weight chemical compounds prevent hydrolytic degradation of ester-containing polymers by consuming moisture and free acid molecules generated during processing. Monomeric carbodiimides act as reactive scavengers in polymers like polyethylene terephthalate or polyurethane. This scavenging prevents the autocatalytic breakdown of the polymer chain.
Reaction Process
The carbodiimide group reacts with carboxyl groups to form stable urea derivatives. This reaction reduces the acid value of the polymer matrix, which halts the acid-catalyzed cleavage of the ester bonds. Adding monomeric carbodiimides during extrusion or injection moulding protects the polymer when it is exposed to humid environments.
The reaction must occur before the resin degrades to preserve mechanical strength.
Volatility Concern
Migration and outgassing during high-temperature melt processing present a challenge with low molecular weight additives. These monomeric carbodiimides can evaporate from the melt during venting or at the nozzle, leading to deposits on the mould. These deposits cause surface defects on the moulded parts and require frequent tool cleaning.
Moulders must monitor venting systems to minimize exposure to the vaporized additives.
Application Boundary
Long-term stability in harsh conditions requires polymeric alternatives with higher thermal resistance. Monomeric grades are best suited for short processing cycles or applications where the part is not exposed to high heat.