Meaning
Surface irregularities or internal voids caused by the presence of water in the polymer melt during processing compromise both the appearance and the mechanical integrity of a part. Moisture defects typically appear in hygroscopic resins such as polyamide or polycarbonate that have not been adequately dried. These flaws result from the rapid expansion of water vapor as the melt exits the nozzle into the atmospheric pressure of the cavity.
Visual Indicator
Silver streaks known as splay represent the most common form of these surface blemishes. When moisture defects occur, the steam bubbles are dragged along the mold wall. This usually leads to rejection.
Structural Degradation
Chemical reactions between water and certain polymers at high temperatures can lead to chain scission. If moisture defects are accompanied by hydrolysis, the impact strength and tensile properties of the material drop notably. Parts may appear visually acceptable but fail under load due to this hidden brittleness.
Molecular weight reduction is a permanent change that cannot be reversed by subsequent cooling.
Processing Cause
Inadequate desiccant performance or saturated air filters often allow wet resin to reach the throat of the press. Because moisture defects are linked to the dew point of the drying air, monitoring the dryer environment is a critical preventative step. Maintaining a dew point of negative forty degrees ensures that the resin remains within the specified parts per million of water.