Meaning
Physical degradation phenomena initiate microscopic cavities within a polymer matrix under applied triaxial tensile stress fields. During mechanical loading or thermal contraction, microvoid nucleation develops around rubber particles, inorganic fillers, or structural inhomogeneities within the solid polymer. The mechanism no longer operates once cavitation transitions into macroscopic crack propagation or unstable brittle fracture.
Cavitation Mechanism
Localized hydrostatic tension triggers volume expansion around embedded rubber domains or rigid mineral particles. Interfacial debonding between matrix and filler lowers the local critical stress required for microvoid nucleation during rapid deformation. Matrix yield stress dictates the onset threshold.
Impact Toughening
Controlled cavitation releases local triaxial stress states and promotes widespread shear yielding across the surrounding polymer resin. High-impact polypropylene and rubber-toughened nylon rely on microvoid nucleation to absorb mechanical energy and prevent catastrophic brittle failure under impact loading. Datasheet notched Izod values indicate the efficiency of this stress relief process in molded test bars.
Excessive regrind content introduces thermal degradation products that trigger premature cavitation at lower stress thresholds, causing premature component failure under load.
Density Reduction
Structural foaming operations exploit deliberate void creation to lower part weight and eliminate sink marks in thick-walled injection molded components. Blowing agents generate dissolved gas concentrations that induce controlled void formation throughout the polymer melt during mould filling.