Meaning
Formation of microscopic cavities between crystalline plates occurs when a semi-crystalline polymer is subjected to tensile stress. As the material stretches, the soft amorphous zones expand and eventually pull apart. While interlamellar voiding is often the first stage of plastic deformation, it can also lead to premature failure if the voids coalesce.
Strain Initiation
Deformation of the spherulitic structure forces the crystalline plates to slide or tilt. During this process, interlamellar voiding appears as the chain segments in the amorphous phase reach their limit of extensibility. This phenomenon is more pronounced in materials with a high degree of crystallinity and a low density of tie molecules.
Optical Alteration
Light scattering from the internal surfaces of the voids causes the material to appear opaque or white. If interlamellar voiding occurs during the bending of a translucent part, the resulting stress whitening acts as a visual indicator of localized overstress. Processors monitor this change to identify areas where part geometry or gate location causes excessive internal strain.
Mechanical Weakness
Voids act as stress concentrators that can initiate larger cracks or crazes. Once interlamellar voiding becomes extensive, the ability of the material to resist further load decreases sharply. Minimizing this effect involves optimizing the cooling rate to ensure a more uniform and durable morphology.