Meaning
Velocity gradients experienced by molten plastic as it is forced through the nozzle, runner, gate, and cavity of a mould. This variable, called injection moulding shear rates, depends on the speed of the injection ram and the thickness of the flow channel. Thermoplastic resins exhibit non-Newtonian flow behavior where viscosity decreases as these shear rates increase.
Designers use this shear-thinning behavior to fill thin-walled parts without requiring excessive injection pressure.
Flow Gradient
Highest shear forces occur near the walls of the runner and gate where the velocity difference between the stationary mould surface and the moving polymer melt is greatest. The center of the flow channel maintains a much lower rate of shear, resulting in a non-uniform viscosity distribution across the melt stream.
Material Degradation
Exceeding the critical shear limit of a polymer resin causes severe chain scission and thermal degradation. This breakdown of the molecular structure results in burn marks, splay, and a significant reduction in the impact strength of the moulded part.
Tooling Constraint
Gate design must balance the need for rapid filling against the risk of high shear. Restrictive gates generate high shear rates that help heat the polymer but can cause jetting if the flow enters the cavity unsupported. Engineers adjust the gate dimensions and injection velocity to keep the local shear rate within the material manufacturer’s recommended limits.