Infrared spectroscopic analysis measures the relative concentration of carbonyl oxidation products present within a polyolefin chain structure. Calculation of the ftir carbonyl index relies on comparing the absorption peak area of oxidized carbonyl groups near 1715 inverse centimetres against an invariant polymer backbone reference band such as the methylene bending peak at 1460 inverse centimetres. The metric quantifies photo-oxidative degradation and thermal aging incurred during outdoor exposure or aggressive reprocessing.
It governs material acceptability in recycled resin streams, stopping short of identifying specific low molecular weight degradation byproducts that require chromatographic separation.
Degradation Baseline
Ultraviolet radiation breaks carbon bonds to generate hydroperoxides that transform into ketones and carboxylic acids. Measuring the ftir carbonyl index reveals early polymer chain scission long before mechanical brittle failure appears in tensile testing. Virgin polyolefin resin exhibits a near-zero initial value.
Recyclate Inspection
Post-consumer regrind batches frequently exhibit elevated oxidation levels due to multiple heat histories during prior processing cycles. Processing heavily oxidized flakes causes melt instability and foul smells during extrusion.
Processing Impact
Thermal degradation shifts molecular weight distribution downward as polymer chains sever under high shear stress. Unstabilized resins display a rapid rise in carbonyl concentration, leading to embrittlement and surface cracking in finished injection moulded parts.