Meaning
Injection moulding flow defects occur when molten polymer slows or halts along thin wall sections while filling thicker adjacent cavities. Severe flow hesitation causes localized thermal loss, leading to premature freezing or incomplete part filling. The flow anomaly governs structural integrity and surface cosmetics in thin-walled electronic housings and complex ribs.
Heat conduction into cold steel walls during the hesitation period sets the boundary where frozen layer growth permanently blocks flow paths.
Rheological Behavior
Polymer melt naturally follows paths of least hydraulic resistance, favoring thick channels over narrow channels. Shear rate inside the narrow channel drops, causing local melt viscosity to increase sharply. Cold resin layers thicken along cavity walls until pressure behind the flow front can no longer overcome fluid friction.
Defect Consequence
Stagnant melt fronts develop thin frozen skins that create visible flow lines or structural weakness upon final packing. Internal stresses concentrate at hesitation boundaries, lowering impact resistance in finished components. Severe stagnation causes short shots in distant rib geometries.
Tooling Adjustment
Modifying wall thickness transitions promotes uniform advancement of the melt front across thin sections. Altering gate location increases local filling velocity, preventing premature freeze-off in restrictive channels. Sequential valve gating controls melt distribution across complex multi-cavity moulds.