Meaning
Dispersed phase structure represents the spatial distribution and shape of the minor polymer component within a continuous polymer matrix. Droplet morphology governs the mechanical properties, barrier efficiency, and surface finish of immiscible polymer blends. The final shape depends on the shear force in the extruder and the interfacial tension between the polymer resins.
Viscous Flow
Deforming forces during compounding stretch the dispersed phase into elongated threads that later break up into smaller spheres. High shear stress in the injection nozzle reduces droplet morphology size, whereas prolonged heating in the mould cavity allows coalescence into larger aggregates. This phase separation can lead to delamination under impact if the interfacial adhesion is weak.
For example, a blend processed with too much regrind material might show irregular domain sizes due to degraded polymer chains, which leads to unstable flow behavior during the injection cycle.
Fracture Resistance
Toughness in the moulded component relies on a fine, uniform distribution of the elastomer phase. If droplet morphology becomes too coarse, cracks propagate through the matrix without being redirected by the rubbery domains. This coarse distribution increases the risk of brittle failure in the finished part.
Viscosity Ratio
Matching the melt flow rates of the two resins at the processing temperature helps minimize domain size. When the viscosity of the dispersed phase is much higher than the matrix, droplet morphology remains large and unevenly distributed. Controlling this ratio ensures consistent impact strength.