Meaning
Removal of solvent molecules from a polymer gel or solution leaves a dry polymer matrix or dense film. This desolvation occurs during solvent casting or recycling processes where a liquid carrier must be evaporated. Solvent concentration changes define the transition from a fluid state to a solid state.
Polymer Precipitation
Phase separation begins when the solvent concentration drops below a critical threshold. During desolvation, the polymer chains move closer together and establish intermolecular bonds that form the solid film structure. If this step happens too quickly, it traps pockets of solvent that cause voids or skin defects in the molded part.
Gradual extraction or drying allows the polymer chains to align into a denser morphology.
Process Control
Temperature and extraction medium flow rates govern the rate of volatile removal. In solvent-cast polymer film production, desolvation must be monitored closely to prevent surface cracking and premature skin formation. High evaporation rates at the surface seal the top layer, which arrests solvent release from the core and extends the cycle time.
Moulders using solvent-welded inserts must also control this rate to ensure the joint achieves full mechanical strength. Proper venting in the extraction zone is necessary to maintain a constant rate.
Material Property
Residual solvent content determines the glass transition temperature and mechanical modulus of the finished polymer. Incomplete desolvation leaves the polymer plasticized, which reduces its tensile strength and increases creep under load. Conversely, complete removal ensures that the material achieves its full rated hardness and thermal stability.
Measuring the weight loss of the extruded film confirms that the process has reached completion.