Meaning
Volumetric displacement of an injection screw during holding and packing stages to the physical mechanical stop of the barrel eliminates the melt reserve required for cavity pressure maintenance. The occurrence of cushion loss indicates that the screw has hit zero position before completion of the holding phase, cutting off pressure transmission to the solidifying cavities. Polymer shrinkage continues inside the tool while the machine cannot deliver compensating material volume, yielding sink marks, vacuum voids and dimensional failure.
The boundary of this condition rests strictly on the injection phase of cycle execution, terminating once the gate freezes and isolation from the runner system occurs.
Forward Position Drift
Uncontrolled forward migration of the screw tip during consecutive cycles signals instability in shot volume metering or mechanical seal decay. When cushion loss manifests across a production run, shot weight exhibits direct downward drift because the final increment of packed melt remains uncompressed in the barrel. The process monitor records zero millimetres remaining before holding time elapses, proving that nominal machine pressure ceased acting on the runner system.
Processing window calculations depend on a constant reserve cushion between two and six millimetres to isolate machine hydraulic fluctuations from tool cavities. Drift into zero cushion exposes the part geometry directly to raw melt compressibility variances.
Melt Starvation
Immediate dimensional underfill and localised gate depression follow when hydraulic pressure drops against the bottomed screw face. Molded components suffer loss of critical rib thicknesses, reduced weld line strength, and pronounced visual sink directly opposite thick wall transitions. Regrind fraction changes accelerate this starvation by introducing variable bulk density in the feed throat, which alters recovery stroke compaction and results in sudden cushion loss during injection.
Virgin resins with narrow molecular weight distributions provide predictable melt compressibility, whereas uncontrolled scrap additions create inconsistent back-pressure dynamics that starve the cavity during high-pressure holding stages. Tool qualification protocols mark any shot exhibiting cushion depletion as an unsalvageable nonconformance.
Check Ring Wear
Mechanical clearance expansion between the non-return valve ring and barrel wall provides an unmetered reverse path for molten polymer under packing pressures. Slippage past a worn sliding ring allows melt to leak back across screw flights during forward motion, transforming an otherwise correct metering stroke into instant cushion loss. Inspecting components for sink defects remains secondary to measuring mechanical clearances inside the barrel once process adjustments fail to stabilise the cushion position.
Worn non-return components require physical replacement rather than elevated holding pressures to restore volumetric holding capability. Continuous cushion depletion under constant dosage volume remains the primary diagnostic marker for check ring erosion.