Meaning
Thermal phenomenon in injection moulding occurs when trapped air within a cavity undergoes rapid reduction in volume without exchanging heat with the surrounding steel. During high-speed injection, adiabatic compression raises the local temperature of the air pocket to several hundred degrees Celsius. This temperature spike can scorch the polymer.
Thermal Effect
Degradation of the polymer chains occurs at the melt front when the compressed gas reaches temperatures above the degradation threshold of the resin. Under these extreme conditions, adiabatic compression causes polymer pyrolysis, leading to localized black spots or weak mechanical bonds. The resulting cosmetic flaws or structural voids can cause the rejection of entire batches of moulded parts.
High heat can also pit the tool steel over time.
Defect Prevention
Adequate venting of the injection mould allows the trapped gas to escape before the advancing melt front can trap and compress it. When venting is insufficient, adiabatic compression produces the diesel effect, which appears as burnt edges or unfilled areas in the part. Machining shallow vent channels along the parting line provides an exit path for the gas.
Vacuum venting systems can also be integrated into the tool to evacuate air before injection starts, ensuring that the cavity is empty before the melt enters.
Process Control
Adjustment of the injection speed profile reduces the velocity of the melt front as it nears the end of the fill stroke. Slowing the ram speed at the end of the stroke allows adiabatic compression to be avoided by giving the air more time to escape. Modern injection moulding machines use multi-stage filling profiles to achieve this precise control.
This approach minimizes burn marks without increasing the overall cycle time.