Meaning
Cumulative percentage of the initial weight of a specimen that is lost through outgassing during a standardized vacuum test. Calculation of the total mass loss provides an overview of the stability of a polymer and its potential to contaminate the surrounding area. This value includes everything that leaves the material, including water vapor and absorbed gases.
Mass Depletion
Heating the sample to 125 degrees Celsius for 24 hours while under vacuum drives the release of volatile components. Although total mass loss indicates how much the material shrinks or lightens, it does not distinguish between harmless water and damaging oils. A high value suggests the presence of many mobile species in the resin, which may lead to physical degradation or the loss of structural integrity over time.
This depletion can result in the part becoming more brittle as the essential additives that provide flexibility are removed from the matrix.
Material Screening
Aerospace standards typically set a maximum limit of one percent for this measurement. If a polymer exceeds this total mass loss threshold, it is generally rejected for use near sensitive electronics or optical paths.
Evaluation Criterion
Comparing the weight before and after the test determines the final percentage. While total mass loss is a useful first pass, it is often paired with measurements of condensable materials to provide a complete picture of risk.