Meaning
Homolytic cleavage of carbon-carbon bonds occurring at elevated processing temperatures cleaves polymer backbones containing active alkyl radical sites. Occurrence of thermal beta-scission reduces molecular weight and melt viscosity in polyolefins during high-temperature extrusion and compounding. Thermal breakdown initiates when peroxide residues or dissolved oxygen generate free radicals along polymer chains.
Unpaired radical electrons prompt backbone cleavage, yielding a terminal olefin fragment and a secondary alkyl radical.
Radical Cleavage
Free radical centers undergo internal electron rearrangement that splits the adjacent carbon-carbon single bond. Rapid cleavage reduces overall polymer chain length without forming volatile light hydrocarbon byproducts. Radical propagation continues until termination reactions pair unreacted species.
Viscosity Reduction
Chain fragmentation lowers melt elasticity and shear viscosity during high-temperature melt processing. Polypropylene producers utilize controlled thermal scission via peroxide addition to tailor melt flow rates for high-speed injection molding grades. Uncontrolled scission degrades resin mechanical strength and flexural modulus.
Scavenger Stabilization
Primary phenolic antioxidants scavenge free radicals to halt propagation steps before chain scission occurs. Secondary phosphite stabilizers decompose hydroperoxides, preventing radical generation during thermal processing. Processor temperature management limits degradation by keeping melt processing conditions within stable operating windows.
Polymer degradation through thermal beta-scission alters molecular weight distribution, directly affecting environmental stress crack resistance in finished components.