Meaning
Propagation of a crack at stress intensity levels below the critical fracture toughness of a material represents a common mechanism for long-term structural failure. Under sustained loads or in aggressive chemical environments, polymer parts can experience subcritical crack growth that gradually weakens the component over time. This slow-growth regime is difficult to detect through visual inspection but leads to sudden catastrophic failure once the crack reaches a critical size.
Failure Mechanism
Mechanisms of slow crack extension in polymers are often driven by a combination of constant mechanical stress and environmental exposure. During this process, polymer chains slowly disentangle and slip past each other at the crack tip, a phenomenon accelerated by the presence of solvents or surfactants. This subcritical crack growth can occur at stress levels far below the yield strength of the resin.
Understanding this behavior is essential for predicting the lifespan of products like pipes or containers that hold pressurized fluids.
Processing Impact
Moulded-in residual stresses from the injection moulding process can act as the primary driver for crack propagation in the absence of external loads. If the melt is cooled too quickly or if the packing pressure is uneven, high internal stresses are locked into the part, predisposing it to subcritical crack growth over its service life. Moulders can reduce these internal stresses by increasing mould temperatures, which allows for slower cooling and more complete relaxation of the polymer chains.
Annealing the moulded parts is another post-processing step used to relieve these harmful stresses.
Material Selection
Resin selection is a primary factor in mitigating the risks of slow failure, as polymers vary widely in their inherent resistance to this phenomenon. High-density polyethylene grades with high molecular weight and a high degree of copolymerization exhibit excellent resistance to subcritical crack growth due to their high concentration of tie molecules. These long chain molecules span the amorphous regions between crystalline lamellae, resisting the disentanglement that allows cracks to advance.
Specifiers must select these optimized grades for applications subjected to continuous loads or chemical exposure.