Meaning
The amount of water remaining in polymer pellets after they have completed the drying cycle determines the risk of hydrolytic degradation during subsequent melt processing. High residual moisture content causes chemical breakdown in hygroscopic resins like nylon and polyester, which leads to weak parts. This water fraction is measured using specialized moisture analyzers before the material enters the molding machine.
Water Fraction
The absolute amount of water is typically expressed in parts per million or as a percentage of the total material weight. When the residual moisture content is too high, the heat of the extrusion process vaporizes the water, creating steam bubbles that can be seen as silver streaks on the surface of the molded parts. These cosmetic defects are often accompanied by a significant reduction in the plastic’s mechanical properties.
This degradation is difficult to detect without mechanical testing, which makes pre process moisture verification essential for quality assurance.
Hydrolysis Risk
At melt temperatures, the water molecules react with the polymer chains, breaking them into smaller segments. This reaction increases the melt flow rate and reduces the molecular weight, which leads to part brittleness. Measuring the residual moisture content ensures that the reaction does not take place.
Drying Practice
To achieve the low levels required for sensitive materials, molders must use desiccant or vacuum dryers. If the resin is exposed to ambient air after drying, it will quickly reabsorb moisture, which renders the drying phase useless. This reabsorption requires that the dried material be kept in sealed hoppers and processed immediately to prevent the moisture levels from rising.